Re: Moderate Boat Oxidation. Wetsand or Buff?
Boat looks good. Luckily the Cobalt is my boat(6 years old n a. BIt neglected so now in recovery mode. The interior seating n top fiberglass are in excellent shape Been buffing cars now tackling boats so use mine to practice. Hooefully i can take one if Mikes classes in the future on gel coat work
-
Re: Moderate Boat Oxidation. Wetsand or Buff?
Originally Posted by PursuitDT
Hey guys/gals,
I inspected a 22ft Four Whinns H210 today for a new client of mine. It has moderate oxidation on the upper portion of the black paint. It's black with a white top. Wish I had photos to share, but that was my mistake. I'm trying to figure out the most efficient way to go about doing this.
Scale 1-10 (10 being really bad)
I would say its a 6-7.
1. Do I wetsand the gel coat down to eliminate the oxidation?
Or
2. Do I buff out the gel coat with my D/A and MF pads? (Keep in mind I do not own a rotary)
I'd like to see if I can get Mike's input on this!
Hope for some feedback.
Thanks.
Not that you can't bring an old thread back to life, but the above was posted,
05-06-2017, 04:54 PM
Originally Posted by Markymapo
Very useful. I have Cobalt 242 that is 6 years old and has moderate oxid (6/7 out of 10)Tried using my flex 3401 with compound/ wool pad test spot (result = it will take me until Christmas 2019 to get it done).
Looks like I either wet sand it or get a rotary n hit with wool/compound.
Will do a wet sand with 3000 grit (least aggressive) using my 3401 and see what happens. Been reading Mikes book n am leaning toward sanding
Here's the deal.... oxidation tends to go INTO the gel-coat so when gel-coat has visible oxidation buffing the surface will restore the shine but it will tend to revert back fairly quickly. Machine sanding will remove all of the oxidation and the results will last longer.
If it's not to bad, then possible Mirka Abralon with #3000 followed by #4000 and then Captain's Compound with a rotary buffer and wool pad. Follow this with the RUPES blue foam coarse pad and the same compound. Then chemically strip and apply Gtechniq C1 Crystal Lacquer.
See picture here,
BEFORE & AFTER - EXTREME Gelcoat Oxidation Removal + Ceramic Coating
See how we did it here,
Pictures: 2018 Boat Detailing Class at Autogeek with Mike Phillips
Next class is February, 9th and 10th 2019 and it's already filling up.
-
Super Member
Re: Moderate Boat Oxidation. Wetsand or Buff?
Learned my lesson not hitting my boat with more passes during wet sanding with 3000 grit thinking I could get the remaining with wool n Captains one step compound n polish. May try 2000 grit followed by 3000, then wool, then polish (test spot). So wanted to take Mike,s class this past winter but my job sent me To China at the same time as his class( the trip was well worth it as I work on developing Oncology drugs). Maybe 2020 I can make the class
2022 Carrera S & Honda CRV Hybrid
2015 Lexus IS 350, 2016 Ford F-150
Cobalt 242 (8.1 L block, Volvo outdrive)
-
Super Member
Re: Moderate Boat Oxidation. Wetsand or Buff?
I ended up going down to 2000 grit, followed by 3000 then wool then foam pad , wow what a work out and still have another side of the boat to do. Just for fun I hit a section with 1000, then 2000, then 3000 then wool then foam pad, but that’s a lot of work. Thanks for the input
2022 Carrera S & Honda CRV Hybrid
2015 Lexus IS 350, 2016 Ford F-150
Cobalt 242 (8.1 L block, Volvo outdrive)
-
Re: Moderate Boat Oxidation. Wetsand or Buff?
Originally Posted by Mike Phillips
Not that you can't bring an old thread back to life, but the above was posted,
05-06-2017, 04:54 PM
Here's the deal.... oxidation tends to go INTO the gel-coat so when gel-coat has visible oxidation buffing the surface will restore the shine but it will tend to revert back fairly quickly. Machine sanding will remove all of the oxidation and the results will last longer.
If it's not to bad, then possible Mirka Abralon with #3000 followed by #4000 and then Captain's Compound with a rotary buffer and wool pad. Follow this with the RUPES blue foam coarse pad and the same compound. Then chemically strip and apply Gtechniq C1 Crystal Lacquer.
Any suggestions for a non skid gel coat surface that is oxidized? It could definitely use some sanding, but the “non skid” is gel coat in the shape of little waves (blue wave pure bay 2400) so sanding would actually damage the non skid. I’ve had amazing results using presta compound, but I’m worried about long term correction and I definitely don’t want to keep going through this.
-
Re: Moderate Boat Oxidation. Wetsand or Buff?
See my reply to your thread.
There’s 3 commonly used types of non-skid
1: Molded-in = gel-coat
2: Painted.
3: Sundeck (could be wrong on this word, I don’t have my book in front of me)
You can machine scrub molded-in as this is gel-coat and it’s tough.
Similar Threads
-
By Mike Phillips in forum PICTURES: 2-Day BOAT Detailing Classes
Replies: 9
Last Post: 12-20-2019, 11:27 AM
-
By Mike Phillips in forum PICTURES: 2-Day BOAT Detailing Classes
Replies: 1
Last Post: 12-10-2019, 03:45 PM
-
By Sonic Pilot in forum Auto Detailing 101
Replies: 12
Last Post: 09-09-2018, 07:44 PM
-
By Mike Phillips in forum PICTURES: Wednesday Night Detailing Classes
Replies: 52
Last Post: 07-09-2014, 11:02 AM
-
By kelley386 in forum Show N' Shine
Replies: 8
Last Post: 05-05-2011, 03:29 PM
Members who have read this thread: 0
There are no members to list at the moment.
Posting Permissions
- You may not post new threads
- You may not post replies
- You may not post attachments
- You may not edit your posts
-
Forum Rules
|
S |
M |
T |
W |
T |
F |
S |
31 |
1
|
2
|
3
|
4
|
5
|
6
|
7
|
8
|
9
|
10
|
11
|
12
|
13
|
14
|
15
|
16
|
17
|
18
|
19
|
20
|
21
|
22
|
23
|
24
|
25
|
26
|
27
|
28
|
29
|
30
| 1 | 2 | 3 | 4 |
|
Bookmarks