I'm not sure if the new version will take care of it but I've heard complaints about ONR as a QD not having any nice slickness to it like most QD's. I've noticed this as well and while it doesn't totally bother me, I figured I'd try something out. I didn't feel like paying almost $40 for the bottle of Polycharger liquid that's suggested for this so I used BFWD instead. I put a few drops, maybe a 1/4 of an ounce or so of my BFWD into a 22 oz bottle of ONR QD. I figured it couldn't really hurt anything so I mixed it, shook it up and tried it. I must say, there is a noticeable slickness now with no adverse effects like streaking or hazing. I was just winging it on the ratio so more can probably be added safely if desired and it should add more of the BF polycharged slickness to what is otherwise a great cleaning detailer. Anybody not happy with the feel of ONR as a QD should give this a shot if they have the BFWD lying around. I figure maybe even adding the wet diamond will give it quick wax properties as well which is always a good thing.