Hey all,
Working on a boat for my cousin. The gelcoat hasn't really been touched since new in 1989. While I can get some great test spots like pictured below, the RUPES 21 with Blue pad & either Meg's 100, 105 or RUPES Zephir do not seem to cut down enough. It won't cut down all of the oxidation. I have also tried Surbuf, Spider & Microfiber pads with multiple combinations of compounds. Even after two times over with the RUPES Blue pad and & M100 (4-6 section passes each time) there is still oxidation left.
Any help or suggestions would be greatly appreciated.