If I get the Flex 3401, and I use the Lake Country 6.5" Gold Jeweling CCS pad, and I use Menzerna PO87MC, at what speed or setting should I use on the Flex to do this? Can it be done effectively with the Flex 3401? Gosh... so many questions, so little time!
Feed back please
Birdhunter
05-14-2009, 07:32 PM
Good Question. Hope someone can answer.
termigator
05-14-2009, 09:07 PM
Good Question. Hope someone can answer.
:whs:
I just finished my '07 Hyundai Sonata with my Flex 3401. I used Wolfgang PPE on an LC blue pad at full speed (6 on Flex) and it yielded a very noticable improvement over the previous Menz FP step (which already was great!). Wolfy's PPE may not be the best product to use for this step but it is what I had on hand - I'll continue to to use it in this fashion because I loved the results!
Regards,
GEWB
If I get the Flex 3401, and I use the Lake Country 6.5" Gold Jeweling CCS pad, and I use Menzerna PO87MC, at what speed or setting should I use on the Flex to do this? Can it be done effectively with the Flex 3401? Gosh... so many questions, so little time!
Feed back please
I use Wolgang Paintwork Polish Enhancer on a blue (or red or black) pad running 5.5 to 6 on the Flex.
See this post, about half way down (search for WPPE):
http://www.autogeekonline.net/forum/show-n-shine/18227-2007-hyundai-sonata-pearl-white.html
Also see:
http://www.autogeekonline.net/forum/auto-detailing-university/18197-can-i-jewel-these-products.html
Regards,
GEWB
Powered by vBulletin® Version 4.2.5 Copyright © 2024 vBulletin Solutions Inc. All rights reserved.