View Full Version : Rusty fitting on foam cannon



DetailRay
04-28-2017, 04:13 PM
Anybody else have this issue? The connector fitting on my CG MTM foam cannon is rusty and probably the reason why the foam is not rich and thick like before. Do they make some kind of rust proof fittings?https://uploads.tapatalk-cdn.com/20170428/d3f81978f1e35df64e9a704a38dc89f4.jpghttps://uploads.tapatalk-cdn.com/20170428/1c8cbe7c7fcbd437a21464dbb41a64f8.jpg

Sent from my SM-G920W8 using Tapatalk

Mp0wer
04-29-2017, 06:47 AM
Just search google for MTM stainless steel quick connects

Eldorado2k
04-29-2017, 08:23 AM
I dealt with this same issue last night...

https://uploads.tapatalk-cdn.com/20170429/e41766ed7c8c591439a5228cc3bd8781.jpg

Not only on the outside, but the inside of the brass fitting was caked as well. I didn't like the idea of what's supposed to be clean rinse water flowing through that, so I took some metal polish and a wire brush to it. Finished it off with some steel wool.

https://uploads.tapatalk-cdn.com/20170429/bf9cf89238180c64293a08962fdd8100.jpg

Then I chiseled the inside clean with a small screwdriver and then brushed it clean with a toothbrush.