Quote:
|
Originally Posted by Whitethunder46 I'm so glad I got OC, it's something slightly stronger than XMT3 and I really needed something like that.
With that said, did you use a yellow pad with OC? I've noticed much more micromarring with OC than XMT3, and was wandering if you did the same? Also, what pad did you then use with XMT1? I've used orange Edge pad with XMT1 after OC/yellow pad, and it's been semi-tough to get out the OC marring. then again, it might just be too cold right now for it to break down correctly.
Did you notice any hiding abilities with the XMT glaze IF there were still any imperfections after polishing?
BTW, the pics look AMAZING! |
I used the yellow pad with the OC But din't get much micro marring, guess that clear coat was like rock. but I used then the XMT1 More for Polish With the Orange Edge, then the glaze was to put some deep wet look to the game, That Car was all around swirl marks, I found it really hard to get rid of them even with the OC, I started with XMT3 but i had to step up to the OC and if i had The Hyper Compound I would've step into that one too.
I spent a long time in every panel I found the OC took to long to break down.
But the temp wasn't so bad over here. Maybe I used too much product.
But at the end everything went ok, and the owner was happy and that's all that matters so time spent was paid off.